The can body remains in front of the weld center
The sharp edge of the roll forming plate scratches paint away. This paint is being welded thereafter in the seam.
The last can is not welded at the end, sometimes the can body remains in the crown.
HMI: all parameters are lost, but the time settings are still there
What to do when the overlap is too big in the beginning and / or too big in the end of each can body?
What are the adjustable parameters of the welding geometry?
My seam has a cold weld towards the end of the can
How to measure the wire correctly
My sheet de-stacker (down stacker) misses feeding body blanks from time to time. What is to do?
The copper wire grooves do not wear straight
What is the "wire elongation" and how much should it be?
I have very irregular seams, what could be the reason?
Roller head & welding machine cooling liquid
Circuit breaker Q5 trips when the machine is switched on or during production